S460NL钢板拉伸屈服及正火冲击分析

S460NL材质是欧标的低合金,执行标准是EN10025

S460NL是正火或者正火轧制,冲击温度为-50°C,在此温度下冲击功值不低于16AKv/J

化学成分:C≤0.20,Si≤0.60,Mn1.00~1.70,P≤0.025,S≤0.020,Ni≤0.80,Cr≤0.30,Mo≤0.10,Cu ≤0.55,Nb≤0.05,V≤0.20,Ti≤0.05,Al≥0.02,N
≤0.025

力学性能:屈服强度以16-40mm为例,拉伸屈服强度不低于440MPa,拉伸抗拉强度在530-720MPa,伸长率A%:17