P265GH/H11拉伸试验/执行标准/对应国内牌号
165GH化学成分丨P265GH力学性能1 P265GH的执行标准为EN 10028-2:2009(E),交货状态为正火。2 化学成分CSiMnPSCrCu≤0.20≤0.400.80-1.40≤0.025≤0.010≤0.30≤0.30MoNbNiTiVNAlt≤0.08≤0.020≤0.30≤0.03≤0.02≤0.012≥0.020备注:Cr+Cu+Mo+Ni≤0.703 力学性能厚度拉伸试验冲击试验屈服强度抗拉强度伸长率%-20℃0℃+20℃≤16265410-5302227344016<t≤4025540<t≤6024560<t≤100215100<t≤150200400-530150<t≤250185390-5304 高温力学性能265GH化学成分丨P265GH力学性能厚度试验温度/℃50100150200250300350400≤1625624122320518817316015016<t≤4024723221519718116615414540<t≤6023722320619017416014813960<t≤100208196181167153140130122100<t≤150193182169155142130121114150<t≤250179168156143131121112105
赞 (0)