Q460EZ35拉伸冲击和化学成分分析

Q460EZ35是国标低合金高强板材质,执行标准为GB/T 1591或者GB/T 16270标准。

冲击温度为-40°C,屈服强度不低于460MPa,抗拉强度550-720MPa

化学成分C ≤0.20, Si≤0.80, Mn ≤1.70, P≤0.02, S≤0.010,Cu≤0.50,Cr≤1.50,Ni≤2.00,Mo≤0.70,B≤0.005,V≤0.12,Nb≤0.06,Ti≤0.05,